Bradt / Tressler

Fractography of Glass

1995. Buch. viii, 302 S.: Bibliographien. Hardcover
Springer ISBN 978-0-306-44880-5
Format (B x L): 15,6 x 23,4 cm
Gewicht: 1370 g
In englischer Sprache
As the first major reference on glass fractography, contributors to this volume offer a comprehensive account of the fracture of glass as well as various fracture surface topography. Contributors discuss optical fibers, glass containers, and flatglass fractography. In addition, papers explore fracture origins; the growth of the original flaws of defects; and macroscopic fracture patterns from which fracture patterns evolve. This volume is complete with photographs and schematics.